Jump to content

File:Stress-Corrosion-Cracking-caused-by-weld-stress-01.jpg

This is a Quality image. Click here for more information.
From Wikimedia Commons, the free media repository
Original file (5,545 × 3,697 pixels, file size: 11.08 MB, MIME type: image/jpeg)

Captions

Captions

Add a one-line explanation of what this file represents

Summary

[edit]
Description
English: Stress corrosion cracking, caused by tension in a unsuitable welded reinforment collar
Deutsch: Spannungsrisskorrosion, verursacht durch nicht spannungsgerechte Schweissung eines Verstärkungskragens
Focus stacking of 14 pictures.
Date
Source Own work
Author CEphoto, Uwe Aranas
Permission
(Reusing this file)

This photo was created by Uwe Aranas. It is protected by law and is not in the Public Domain. However, it can be used free of charge by everyone under the terms of the license stated below.

  • The requirements to comply with the terms of licence are:
- The image is credited with "Photo by CEphoto, Uwe Aranas" or alternatively with "© CEphoto, Uwe Aranas" in close relation to the image. If this is not possible due to shortage of space, please contact me first.
- You are required to release the image under the same license.
  • Not required by the license but highly appreciated:
- Set up a weblink to the original image when you use the image in online media: https://commons.wikimedia.org/wiki/File:Stress-Corrosion-Cracking-caused-by-weld-stress-01.jpg
- Send me a specimen copy or a pdf when used in print media or the URL of the website where the image is used.

Please write an email to spam@aranas.de (where you substitute the word spam by cephoto2020), if you

  • need the image in a higher resolution
  • need my postal address for sending a specimen copy
  • have further questions to the terms of licence
Attribution
(required by the license)
InfoField
Photo by CEphoto, Uwe Aranas / 
Photo by CEphoto, Uwe Aranas

Do not upload new revisions over this file version without my explicit consent. Instead, use the possibility to upload a new version under a new name and tag it as a derivate or extract of this file.

This image has been assessed using the Quality image guidelines and is considered a Quality image.

العربية ∙ جازايرية ∙ беларуская ∙ беларуская (тарашкевіца) ∙ български ∙ বাংলা ∙ català ∙ čeština ∙ Cymraeg ∙ Deutsch ∙ Schweizer Hochdeutsch ∙ Zazaki ∙ Ελληνικά ∙ English ∙ Esperanto ∙ español ∙ eesti ∙ euskara ∙ فارسی ∙ suomi ∙ français ∙ galego ∙ עברית ∙ हिन्दी ∙ hrvatski ∙ magyar ∙ հայերեն ∙ Bahasa Indonesia ∙ italiano ∙ 日本語 ∙ Jawa ∙ ქართული ∙ Qaraqalpaqsha ∙ 한국어 ∙ kurdî ∙ кыргызча ∙ Latina ∙ Lëtzebuergesch ∙ lietuvių ∙ македонски ∙ മലയാളം ∙ मराठी ∙ Bahasa Melayu ∙ Nederlands ∙ ਪੰਜਾਬੀ ∙ Norfuk / Pitkern ∙ polski ∙ português ∙ português do Brasil ∙ rumantsch ∙ română ∙ русский ∙ sicilianu ∙ slovenčina ∙ slovenščina ∙ shqip ∙ српски / srpski ∙ svenska ∙ தமிழ் ∙ తెలుగు ∙ ไทย ∙ Tagalog ∙ toki pona ∙ Türkçe ∙ українська ∙ oʻzbekcha / ўзбекча ∙ vèneto ∙ Tiếng Việt ∙ 中文 ∙ 中文(简体) ∙ 中文(繁體) ∙ +/−

Licensing

[edit]
I, the copyright holder of this work, hereby publish it under the following license:
w:en:Creative Commons
attribution share alike
This file is licensed under the Creative Commons Attribution-Share Alike 3.0 Unported license.
Attribution:
Photo by CEphoto, Uwe Aranas or alternatively © CEphoto, Uwe Aranas
You are free:
  • to share – to copy, distribute and transmit the work
  • to remix – to adapt the work
Under the following conditions:
  • attribution – You must give appropriate credit, provide a link to the license, and indicate if changes were made. You may do so in any reasonable manner, but not in any way that suggests the licensor endorses you or your use.
  • share alike – If you remix, transform, or build upon the material, you must distribute your contributions under the same or compatible license as the original.

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current19:20, 1 April 2015Thumbnail for version as of 19:20, 1 April 20155,545 × 3,697 (11.08 MB)Cccefalon (talk | contribs)=={{int:filedesc}}== {{Information |description={{en|1=Stress corrosion cracking, caused by tension in a unsuitable welded reinforment collar}}{{de|1=Spannungsrisskorrosion, verursacht durch nicht spannungsgerechte Schweissung eines Verstärkungskragen...

File usage on other wikis

The following other wikis use this file:

Metadata